Axiall 5055 Rigid PVC, Extrusion, White

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 5055 Rigid PVC, Extrusion, White.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor WeatherabilityInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D-785
Hardness, Shore D 81
81
ASTM D-2240
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Tensile Modulus 2.97 GPa
431 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.79 GPa
404 ksi
ASTM D-790
Izod Impact, Notched 9.08 J/cm

@Thickness 6.35 mm
17.0 ft-lb/in

@Thickness 0.250 in
ASTM D-256
12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Dart Drop Total Energy 147 J/cm
0.275 ft-lb/mil
H.25 Tup, Method A; ASTM D-4226
Thermal Properties Metric English Comments
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Descriptive Properties Value Comments
Cell Classification 14423433
ASTM D-4216