Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.5 MPa | 3700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPH-20C UV Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | >= 25.5 MPa | >= 3700 psi | ASTM D638 |
S&E Specialty Polymers TufGuard M™ GPP1001M-P-2986 Grey PP, Flame Retardant Application: High impact resistant, non-blooming flame retardant polypropylene compound designed for UL94 V-0 injection molding applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-1902 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
Hyosung Topilene C600M PP C600M Film Grade Butane Random CopolymerApplications: Metallizing CPPCharacteristics:Low sealProcessabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 25.5 MPa @Thickness 3.20 mm |
3700 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL EI5002 PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 9002-88-4Information provided by LG Chemical |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
Global J-2308 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in/min (50 mm/min); ASTM D-638 |
Ineos HP53-25-155 HDPE HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
Lotte Chemical Titan TITANZEX® HM5000 High density polyethylene HM5000 is a high density polyethylene for extrusion monofilament. HM5000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3... |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
LyondellBasell Petrothene® LP5100 High Density Polyethylene ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist.. |
|||
Tensile Strength, Yield | 25.5 MPa @Thickness 3.20 mm |
3700 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HI5302S PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
Techmer ES Luriblend® PE 5902 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
Techmer ES HiFill FR® PP FR-N X Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S368D Thermoplastic Polyurethane Type: Estane® S368D is a Shore 68D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
A. Schulman PP 3353-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 3353-01 is a high flow medium impact polypropylene which is suitable for molding thin parts with long mold flow distances. It permits reduction of cycle times, temperatu.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | at max load; ASTM D638 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in/min; ASTM D638 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in/min; ASTM D638 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
A. Schulman PP 3353-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 3353-01 is a high flow medium impact polypropylene which is suitable for molding thin parts with long mold flow distances. It permits reduction of cycle times, temperatu.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
ExxonMobil HDPE HD 6719.62 High Density Polyethylene Copolymer Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | ASTM D638 |
Amco Amalloy® B9714 Polymer Alloy Amco Amalloy B9714 is a clear performance copolymer with exceptional clarity and toughness.High elongation before breakage, good melt Flow.Information provided by Amco Plastic Materials. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in/min; ASTM D638 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in/min (50 mm/min); ASTM D-638 |
Ineos J50-1000-181 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin c.. |
|||
Tensile Strength, Yield | 25.5 MPa | 3700 psi | 2 in/min.; ASTM D638 |
Ineos J50-1000-187 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin con.. |