Polymer Property : Tensile Strength, Yield = 3700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ FR PP 307 Polypropylene, Unspecified (PP, Unspecified)
Information provided by PolyOne
Tensile Strength, Yield >= 25.5 MPa
>= 3700 psi
ASTM D638
S&E Specialty Polymers GPP1001M-P-2986 Grey PP
Application: High impact resistance, non-blooming flame retardant polypropylene compound for UL94-V0 injection molding applications.Information provided by S&E Specialty Polymers
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in per min; ASTM D638
Network Polymers NPP 25-1902
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
PolyMirae Moplen EP300L Injection Molding Grade Polypropylene
Moplen EP300L is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300L is a block copolymer selected by customers for use in in..
Tensile Strength, Yield >= 25.5 MPa
>= 3700 psi
Kazanorgsintez 276-288 High Density Polyethylene Composite
Production Method: Compositions are achieved by gaseous-phase method. Application: Composition is intended for production of polymer film fibers contacting bulk food.Information Provided by Kaza..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Hyosung Topilene C500H PP
C500H Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Hyosung Topilene C600H2 PP
C600H2 Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Ineos T50-1000 HDPE Copolymer
T50-1000 is a high density polyethylene copolymer. It has a narrow molecular weight distribution and provides injection molded parts with an excellent balance of properties and processing for most g..
Tensile Strength, Yield 25.5 MPa
3700 psi
50mm/min; ASTM D638
LG Chemical SEETEC M1400 Polypropylene Impact Copolymer
Features: SEETEC M1400 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1400 exhibits a high flowability and a good balance of stiffness and impact strength. SEE..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
LyondellBasell Petrothene® LP5100 High Density Polyethylene
ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Global S-5000 High Density Polyethylene
Description-good for monofilament Applications-ropes, fishing net, agricultural net and sports netInformation provided by Global Polymers Corporation.
Tensile Strength, Yield 25.5 MPa
3700 psi
2in/min; ASTM D638
Styrolution Styrolux® 3G46 SBC
Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Techmer ES HiFill FR® PP FR-N X
Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: Natural ColorInformation provided by TP Composites, Inc.
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
A. Schulman PP 3353-01 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 3353-01 is a high flow medium impact polypropylene which is suitable for molding thin parts with long mold flow distances. It permits reduction of cycle times, temperatu..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Plastics Group Polifil® RP-PP Polypropylene, Black
Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low de..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene
DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min; ASTM D638
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene
DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman.
Tensile Strength, Yield 25.5 MPa
3700 psi
2" (50mm) per min; ASTM D638
Formosa Plastics Formolene® 3435E Random Copolymer Polypropylene
Random Copolymer for Clear Storage Boxes, Pill Vials and Containers Formolene® 3435E is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for injection mo..
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min; ASTM D638
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc..
Tensile Strength, Yield 25.5 MPa
3700 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.0 PHR Caytur 4
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 25.5 MPa
3700 psi
at 300% elongation; ASTM D412
Lubrizol Estane® R198A-8 Thermoplastic Polyurethane
Type: Estane® R198A-8 is a Shore 98A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Information Provided by The Lubri..
Tensile Strength, Yield 25.5 MPa
3700 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min; ASTM D638
ExxonMobil PP7684KN Impact Copolymer
Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance ..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Amco Amalloy® B9714 Polymer Alloy
Amco Amalloy B9714 is a clear performance copolymer with exceptional clarity and toughness.High elongation before breakage, good melt Flow.Information provided by Amco Plastic Materials.
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Aaron Industries AAROLENE® ARPP 200-2 PP Black Polypropylene Copolymer
AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A high flow polypropylene copolymer resin, pre-colored black, specifically designed for all high speed injection molding applicati..
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min (50 mm/min); ASTM D-638
Ineos J50-1000-181 HDPE
A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin c..
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..