Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.0 MPa | 2470 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JLK51A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min; ISO 527 |
Mytex Polymers AS88L-01 Polypropylene, Compounded, Elastomer Description: AS88L-01 is a compounded, elastomer modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications .. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, 589 Blue OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, DG OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, W OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2/1A |
Polymer Industries Polyslick UHMW Profile Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527 |
GEHR Plastics PE-UHMW-ELS Polyethylene
(discontinued **) Polyethylene offers resistance to almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature of HDPE is from -58 °F to +1.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | |
Kazanorgsintez PE80B-286 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
LG Chemical LUPOL TE-5202U Thermoplastic Elastomer Alloy, 20% Polymer Alloy, High Impact, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Kostat BK-STAT BK-STAT is an inherently dissipative polymer incorporated into a variety of resins as a melt additive. The electrical resistivity is reduced by formation of a conductive percolating network in the .. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Ineos Styrenics Polystyrene 486N (NAFTA) High-impact grade of polystyrene with excellent ESCR.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-1, -2 |
LyondellBasell Hifaxâ„¢ CA1110/2AC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA1110/2AC Black medium high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a very good balance of processability, impact.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good sur.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527 |
Unipetrol PE HD LITEN® SB/SL 20 HDPE Made for blow molding, tubular film and special applications.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 300 % |
2470 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8792A S043 Polyurethane PreprocessingMax. Water content |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2 |
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437T10L1 Talc Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437T20L1 Talc Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W10L Wollastonite Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W20L1 Wollastonite Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527 |
Azoty Tarnow™ TARFLEN SM-B40 PTFE Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527 |
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527 |
Total Finacene® BM359SG HDPE, blow molding
(Unverified Data**) FINACENE® BM359 SG has been especially designed for the manufacture of blow moulded bottles (up to 5 liters) with a superior surface gloss and contact transparency. It is recommended either in mono.. |
|||
Tensile Strength, Yield | 17.0 - 37.0 MPa | 2470 - 5370 psi | Average value: 29.8 MPa Grade Count:12 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |