Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kostat BK-STAT

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Kostat
Trade Name BK-STAT
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kostat BK-STAT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BK-STAT is an inherently dissipative polymer incorporated into a variety of resins as a melt additive. The electrical resistivity is reduced by formation of a conductive percolating network in the host resin. This is a permanent, non-migratory anti-static agent. This additive is also thermally stable and effective at low humidity levels.The recommended use levels are 10-25% and surface resistivity of E8-12 ohms/square can be achieved.Special Features:Superior Permanent Static DissipationHumidity InsensitivityNo Particle GenerationNo MigrationExcellent ColorabilityGood ProcessibilityApplications:Semiconductor PackagingLCD PackagingElectrical & ElectronicsMedical DevicesStorage DisksAppliancesConsumer GoodsClean Room Accessories
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 200 °C
20 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM D638
Flexural Strength 5.40 MPa
783 psi
ASTM D790
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+8 ohm
1.00e+8 ohm
ASTM D257
Static Decay <= 0.020 sec
<= 0.020 sec
5kV to 50V; FTMS 101C
Processing Properties Metric English Comments
Drying Temperature 50.0 - 60.0 °C
122 - 140 °F
Dry Time 2 - 3 hour
2 - 3 hour
Users viewing this material also viewed the following: