Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ASTM D638 |
Ovation Polymers Optrene 10GF Polypropylene Chemically coupled glass reinforced(10%) polypropylene with high strength and HDT.Information provided by Ovation Polymers |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min |
Polimeri Europa SINKRAL B260 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-04-09-25 Very high heat injection moulding grade with good impact resistance for this category of ABS. Main.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ISO R527 |
Fainplast Compounds RI 528/H Rigid PVC, Antishock Injection Molding Road drains |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ISO R527 |
Fainplast Compounds RKS 300 Rigid PVC, Antishock Extrusion Lead Free Dielectric conduits, antishock |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 150°C for 1,000 hrs; ASTM D1458 |
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific) LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 303 Natural FA PA66, Conditioned Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe Product Applications: TECHNYL® A 303 Natural FA offers three main advantages: high impact resista.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+PS LNP* Lubricomp* Noryl_SPN422L compound is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Valox® 357 PBT PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
Styrolution Terlux® 2802 HD MABS Description: Terlux 2802 HD is a standard injection molding Methyl Methacrulate Acrylonitrile Butadiene Styrene grade for transparent parts.Information provided by STYROLUTION, which is a joint vent.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 2 in/min; ASTM Test |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50mm/min; ISO 527-1/-2 |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ASTM D638 |
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific) 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D 638 |
Cossa Polimeri ESTADIENE 1030 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good impact resistance, high gloss, good light resistance, good processabilityInformation provided by Cos.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
Chi Mei Kibilac® PW-997S ASA Polymer Extrusion |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min |
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Dry) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ISO 527-1 |
Barlog Plastics KEBAFORM C 902 TF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
BASF Ultramid® BU50I BK 106 PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I BK-106 is an unreinforced PA6, impact modified, pigmented black, injection molding product that maintains its impact strength and ductility to -40 deg F .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
Ashley Polymers Ashlene® L930 Nylon 12 A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. The natural color is slightly darker.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50mm/min; ISO 527 |
BASF Ultramid® 8281 HS PA6 (Dry) |
|||
Tensile Strength, Yield | 48.0 MPa @Temperature 23.0 °C |
6960 psi @Temperature 73.4 °F |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers. |