Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ASTM D 638 |
Polimeri Europa Sinkral® F 332 ABS Resin Sinkral F 332 is a general purpose injection molding grade which combines excellent thermal stability during processing with a good balance between flow and impact characteristics. Designation: Ther.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ASTM D638 |
Ovation Polymers OpteSTAT™ NC PP 0030 Polypropylene based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | |
Radici Radilon® S 40E (cond.) Nylon 6 PA6 high viscosity injection molding suitable also for extrusion.Information provided by Radici group. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min |
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Strength, Yield | 42.0 - 98.1 MPa | 6090 - 14200 psi | Average value: 67.9 MPa Grade Count:17 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
Gichem GILAC H120X6/VOU ABS Flame Retardant
(discontinued **) ABS self-extinguishing class V0 with better fluidity and UV resistance. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO R527 |
Fainplast Compounds RH 212/W Rigid PVC, Antishock Extrusion Outdoor antishock profiles |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO R527 |
Fainplast Compounds RKI 0822 Rigid PVC, Antishock Injection Molding Lead Free Technical items |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO R527 |
Fainplast Compounds RKS 212/W Rigid PVC, Antishock Extrusion Lead Free Outdoor antishock profiles |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific) LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DP003F PC LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ISO 527-1/-2 |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527-1/-2 |
Styrolution Terlux® 2812 HD MABS Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
UBE UMERIT 500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
Aclo Accucomp ABS ABS810L Medium Impact Grade |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437G20CL Glass Reinforced Coupled |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50mm/min; ASTM D638 |
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min |
Arkema Group Oroglas® SG 10 Acrylic, Gamma Radiation Resistant
(discontinued **) OROGLAS SG 10 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no advers.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
BP Amoco Accpro® 9961 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: NucleatedTypical applications: CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min |
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |