Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.9 MPa | 5500 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-000/18T 2S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-10GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass/Carbon Fiber Filled
(discontinue Description/Features:Glass/Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 37.9 - 53.4 MPa | 5500 - 7750 psi | Average value: 45.0 MPa Grade Count:41 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Yield | 37.9 - 50.4 MPa | 5500 - 7310 psi | Average value: 42.9 MPa Grade Count:8 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | |
Ineos ABS Centrex® 811 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
M. Holland Company PP200 Polypropylene Homopolymer High ESCRGood heat aging resistanceHomopolymerGood stiffnessApplications: AutomotiveHospital goodsHousehold goodsTable products |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
M. Holland Company PP410 Polypropylene Homopolymer AntistaticMedium flowGeneral purposeHomopolymerNucleatedApplications: Food containersGeneral purposeHousehold goodsToys |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Global ABS-405 FR High Impact, Flame Retardant ABS Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Global ABS-FR0 High Impact, Flame Resistant ABS Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 37.9 MPa @Temperature 23.0 °C |
5500 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H12Z-00 Polypropylene Homopolymer This is a nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Appl.. |
|||
Tensile Strength, Yield | 37.9 MPa @Temperature 23.0 °C |
5500 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H20Z-00 Polypropylene Homopolymer This is a nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Appl.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information .. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Spartech Acrylloy 10 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D-882 |
Saint-Gobain Norton® UHMW PE Skived PTFE Film Description: UHMWPE = ultra-high molecular weight polyethylene; PTFE = polytetrafluoroethyleneApplications include: Common in Protective/Decorative ApplicationsInformation provided by Saint Gobain P.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM Data |
Styron Magnum™ 347EZ ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D412 |
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy Elastomeric Stat-Rite® Polymer alloy X-5065 blend is a patented inherently dissipative polymer (IDP) with thermoplastic polyurethanes (TPU). This produces soft, flexible polymer alloys with an in.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA S750 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D-638 |
Axiall SP-6655 Rigid PVC, Molding Georgia Gulf SP-6655 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, good melt flow, and exceptional.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D-638 |
Axiall UV-6685 Rigid PVC, Molding Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation.Info.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D-638 |
Bapolene® 4062NA Polypropylene, Injection Grade Bapolene 4062NA is a homopolymer polypropylene designed for fast-cycle molding. It is nucleated and contains antistat. This product meets FDA 21CFR177.1520.Applications: Rigid packaging, housewares.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Asahi Kasei Thermylene® P-05FG-0870 5% Glass Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D-638 |
Bapolene® 4082NA Polypropylene Bapolene 4082NA is a homopolymer polypropylene designed for fast-cycle molding applications. It is nucleated and contains antistat. Material meets the requirements of US FDA 21 CFR1777.1520.Applic.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH200LN-02 Polypropylene, Homopolymer, Rx grade, Nucleated, Lube, Injection Molding COPYLENE™ CH200LN-02 is a polypropylene homopolymer resin nucleated for faster crystallization with antistatic properties and designed for injection molding applications. Applications: Caps & Closu.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-25GB/5T-2S Acetal-Copolymer, Glass Bead Filled, PTFE/Silicone Lubricated
(discontinued Description/Features:Glass Bead FilledPTFE/Silicone LubricatedInformation provided by PolyOne Corporation. |