Material Notes:
Description: Flame Retardant SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
ASTM D638
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Unnotched 6.41 J/cm
12.0 ft-lb/in
ASTM D256
0.534 J/cm

@Temperature -40.0 °C
1.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 55.6 J
41.0 ft-lb
73°F; ASTM D3029
27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 75.6 µm/m-°C

@Temperature 20.0 °C
42.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM D648
Flammability, UL94 V-0
V-0
5V
Optical Properties Metric English Comments
Gloss 20 %
20 %
Gardner; ASTM D2523