Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills P4C5B-075 Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: tape extrusion and closures.Former Huntsman polypropylene products are now prod.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills P4C5B-076 Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: cutlery and closuresFormer Huntsman polypropylene products are now produced by .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
IRPC Polimaxx Polene 1102K Polypropylene Homopolymer CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS:MONOFILAMENT/YARN/SHEET EXTRUSION AND INJECTION MOLDING COARSE TEXTILE FOR WOVEN BAGS, TARPAULINS, ROPES, STRAWS, INDUSTR.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-1/-2 |
Mitsubishi Xantar® SF 22 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Kostat BK-STAT 7048BK ABS Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
IRPC Polimaxx Polene 1202J Polypropylene Homopolymer CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS: MONOFILAMENT/YARN/SHEET EXTRUSION AND INJECTION MOLDING COARSE TEXTILE FOR JUMBO BAGS, ROPES, STRAWS, SHEETS, INDUSTRIAL.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ZI001 PPE+PS LNP* LUBRICOMP ZI001 is a compound based on PPE+PS resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS (Asia Pacific) LNP* Thermocomp* AX08306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Mineral. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PN235 PPE+PS Plating grade, primarily automotive applications. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PN235 PPE+PS (Asia Pacific) Plating grade, primarily automotive applications. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Total PPH 12020 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 12020 is a clarified high fluidity homopolymer with a melt flow index of 60 g/10 min.Polypropylene PPH 12020 has been designed with a very high stiffness and an outstanding transpa.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Total PPH 3740WR Polypropylene, High Flow Nucleated Homopolymer Injection Molding Easy Flow TOTAL Polypropylene 3740WR exhibits exceptionally easy flow characteristics.FDA. 3740WR complies with all applicable FDA and USDA regulations and may be used under these provisions for .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Denka MALECCA K-700 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Denka MALECCA K-600 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Aclo Accuguard Polypropylene HP0362V0CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Braskem H 107 Coating Polypropylene Description: H 107 is a ultra-high melt flow rate additivated homopolymer used for general purposes. Designed for extrusion coating. This product exhibits excellent processability, good melt stabili.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336T10L1 Talc Reinforced |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339T10L1 Talc Reinforced |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
Unipetrol PP MONSTEN® FK 005 Polypropylene Homopolymer Applications include injection molding and thermoforming. Antistatic stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Braskem H 605 Extrusion Polypropylene Description: H 605 is a low melt flow rate homopolymer with high transparency. This resin is designed for extrusion and thermoforming. H 605 exhibits excellent processability, high output, excellent.. |