Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NI-0920063 NATURAL Polyamide 610 (Nylon 610) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 600 A 33 Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PK-30GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ ND633 GF Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PK-30GF/000 HT Polyaryletherketone, Glass Filled
(discontinued **) Description/Features:30% Glass FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527-2/1A/5 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527 |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2310F PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF33 L RD041 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: YellowTPCI# 8221102Information provi.. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF25 HS L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF27 SL2 27% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 27% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 HS L BK 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 L BKN001 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Techmer ES HiFill® PA6 B3 EG6 MB Colors Availability: North AmericaForms: PelletsAppearance: Colors AvailableTPCI# 6101102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Techmer ES HiFill® PPA GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu.. |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Clariant Renol 60G33-L Nylon 6, 33% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Clariant Renol PA213G33 Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 165 MPa | 24000 psi | ASTM D638 |
Clariant Renol PPSSP0008 Polyphenylene Sulfide, Carbon Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | |
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |