Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | |
Westlake LF2040 Hexene Linear Low Density Polyethylene Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | |
Westlake LF2050 Hexene Linear Low Density Polyethylene Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05CH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018MK Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LD 102.LC Thin Gauged Film Resin L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and .. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawn down to thing gauges.Availability: Latin America, North America and S.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LL 1001x26 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LL 1001x72 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LL 1001x74 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LL 1001x76 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
Dow FLEXOMER™ ETS-9064 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
Dow FLEXOMER™ ETS-9064 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, MD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |