Material Notes:
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Enable 20-10 resins are available for blown film, both formulated and non-formulated. A heavily stabilized formulation for cast film processing is also available.Availability: Latin America, North America and South AmericaAdditive: Antiblock: No Slip: No Processing Aid: Yes Thermal Stabilizer: YesApplications:Agricultural FilmBlown FilmCast FilmCast Stretch Film Food packagingForm Fill and Seal PackagingHeavy Duty BagsLamination FilmMultilayer Packaging FilmShrink FilmStand Up PouchesStretch FilmInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa
1500 psi
ASTM D882
Film Elongation at Break, MD 520 %
520 %
ASTM D882
Film Elongation at Break, TD 730 %
730 %
ASTM D882
Puncture Energy 3.05 J
2.25 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 120 g
120 g
ASTM D1922
Elmendorf Tear Strength TD 560 g
560 g
ASTM D1922
Dart Drop Test 190 g
0.419 lb
ASTM D1709A
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
1% Secant Modulus, MD 207 MPa
30000 psi
ASTM D882
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 7.1 %
7.1 %
ASTM D1003
Gloss 61 %
61 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 10 lbf
ExxonMobil Method