Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexi.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D 882 |
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FF 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FF 106 are characterized by .. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LGH 138 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 138 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, slip agent, antiblocking and processing aid, suitable for blown film extrusion.Films obtai.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion, food and liquid packaging.Data provided by the manufacturer.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufactur.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 20075AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 3.1 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0318-E Butene LLDPE Film Resin PF-0318-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ISO 527-3 |
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | |
Dow DOWLEX™ 2267A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2267A Polyethylene resin is a high performance blown film polymer offering superior load retention and toughness for a variety of stretch film packaging applications. This material complies.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | |
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
Bapolene® 222F Polyethylene, Film Grade Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
Westlake Hifor Xtreme SC74860-F Polyethylene
(discontinued **) Hifor Xtreme Polyethylene SC74860-F is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more conventional 2.0-2.5 MI cas.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |
|||
Film Tensile Strength at Yield, MD | 9.00 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufacturer. |