Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66  (Unverified Data**)
Zytel® 103FHSA NC010 is a heat stabilized, lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66  (Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66  (Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® E41HSB NC010 Nylon 66  (Unverified Data**)
Zytel® E41HSB is an unreinforced, high viscosity, heat stabilized polyamide 66 for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Zytel® E51HSB NC010 is a high molecular weight, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66  (Unverified Data**)
Zytel® E53 NC010 is a very high viscosity polyamide 66 resin for extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 55.0 MPa

@Temperature 150 °C
7980 psi

@Temperature 302 °F
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:..
Tensile Strength, Yield 55.0 MPa

@Temperature 982 °C
7980 psi

@Temperature 1800 °F
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel
Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated..
Tensile Strength, Yield 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66  (Unverified Data**)
Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D..
Tensile Strength, Yield 55.0 MPa

@Strain 0.200 %,
Temperature 982 °C
7980 psi

@Strain 0.200 %,
Temperature 1800 °F
Solution Annealed Tubing
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..