Mechanical Properties Metric English Comments
Tensile Strength, Yield 420 MPa

@Strain 0.200 %,
Temperature 100 °C
60900 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4021 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Tensile Strength, Yield 420 MPa

@Strain 1.00 %,
Temperature -80.0 °C
60900 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 420 MPa

@Strain 1.00 %
60900 psi

@Strain 1.00 %
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, and rod forms.
Tensile Strength, Yield 420 MPa

@Strain 0.200 %
60900 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu 4565 High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Yield 420 MPa

@Strain 0.200 %,
Temperature 150 °C
60900 psi

@Strain 0.200 %,
Temperature 302 °F
EN min.; EN 10002-5
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Yield >= 420 MPa

@Strain 0.200 %
>= 60900 psi

@Strain 0.200 %
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54
Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl..
Tensile Strength, Yield 420 MPa

@Temperature 93.0 °C
60900 psi

@Temperature 199 °F
Dry
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric
Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3kInformation provided by HexCel
Tensile Strength, Yield >= 420 MPa

@Strain 0.200 %,
Thickness 80.0 - 115 mm
>= 60900 psi

@Strain 0.200 %,
Thickness 3.15 - 4.53 in
Temper T451; Standard EN 485-2
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..
Tensile Strength, Yield >= 420 MPa

@Strain 0.200 %,
Thickness 60.0 - 80.0 mm
>= 60900 psi

@Strain 0.200 %,
Thickness 2.36 - 3.15 in
Temper T651; Standard EN 485-2
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength, Yield 420 MPa

@Strain 0.200 %,
Thickness 450 - 700 mm
60900 psi

@Strain 0.200 %,
Thickness 17.7 - 27.6 in
long-transverse direction
Constellium Alumold® 500 Forged Aluminum
Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to ..
Tensile Strength, Yield 420 MPa

@Strain 0.200 %,
Thickness 450 - 700 mm
60900 psi

@Strain 0.200 %,
Thickness 17.7 - 27.6 in
Typical Strength
Constellium Certal® SPC Forged Aluminum
Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property..
Tensile Strength, Yield >= 420 MPa

@Strain 0.200 %,
Thickness 50.0 - 100 mm
>= 60900 psi

@Strain 0.200 %,
Thickness 1.97 - 3.94 in
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Tensile Strength, Yield >= 420 MPa

@Strain 0.200 %,
Thickness 60.0 - 80.0 mm
>= 60900 psi

@Strain 0.200 %,
Thickness 2.36 - 3.15 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..