Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 245 MPa @Strain 0.200 %, Temperature 50.0 °C |
35500 psi @Strain 0.200 %, Temperature 122 °F |
EN min.; EN 10002-5 |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Yield | 245 MPa @Strain 0.200 % |
35500 psi @Strain 0.200 % |
Typical after Solution Annealing |
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi.. |
|||
Tensile Strength, Yield | 245 MPa @Strain 0.200 % |
35500 psi @Strain 0.200 % |
Typical after Solution Annealing |
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r.. |
|||
Tensile Strength, Yield | >= 245 MPa @Strain 1.00 % |
>= 35500 psi @Strain 1.00 % |
|
Industeel URANUS® 65 310 L Modified Grade - Low C and Si for Nitric Acid Service Description: URANUS® 65 is a 25 Cr 20 Ni austenitic stainless steel with sharp control of the residual elements in order to provide high corrosion resistance properties in boiling 50-65% Nitric a.. |
|||
Tensile Strength, Yield | >= 245 MPa @Strain 0.200 % |
>= 35500 psi @Strain 0.200 % |
|
Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Tensile Strength, Yield | >= 245 MPa @Strain 0.200 % |
>= 35500 psi @Strain 0.200 % |
|
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Tensile Strength, Yield | >= 245 MPa @Strain 0.200 %, Thickness 40.0 - 60.0 mm |
>= 35500 psi @Strain 0.200 %, Thickness 1.57 - 2.36 in |
Temper T451; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Tensile Strength, Yield | 245 MPa @Thickness 19.1 mm, Temperature 316 °C |
35500 psi @Thickness 0.752 in, Temperature 601 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Tensile Strength, Yield | 245 MPa @Strain 0.200 %, Temperature 760 °C |
35500 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |