Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 420 MPa @Strain 0.200 %, Temperature 100 °C |
60900 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Tensile Strength, Yield | 420 MPa @Strain 1.00 %, Temperature -80.0 °C |
60900 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 420 MPa @Strain 1.00 % |
60900 psi @Strain 1.00 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, and rod forms. |
|||
Tensile Strength, Yield | 420 MPa @Strain 0.200 % |
60900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 420 MPa @Strain 0.200 %, Temperature 150 °C |
60900 psi @Strain 0.200 %, Temperature 302 °F |
EN min.; EN 10002-5 |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Tensile Strength, Yield | >= 420 MPa @Strain 0.200 % |
>= 60900 psi @Strain 0.200 % |
|
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54 Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl.. |
|||
Tensile Strength, Yield | 420 MPa @Temperature 93.0 °C |
60900 psi @Temperature 199 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3kInformation provided by HexCel |
|||
Tensile Strength, Yield | >= 420 MPa @Strain 0.200 %, Thickness 80.0 - 115 mm |
>= 60900 psi @Strain 0.200 %, Thickness 3.15 - 4.53 in |
Temper T451; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Tensile Strength, Yield | >= 420 MPa @Strain 0.200 %, Thickness 60.0 - 80.0 mm |
>= 60900 psi @Strain 0.200 %, Thickness 2.36 - 3.15 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Tensile Strength, Yield | 420 MPa @Strain 0.200 %, Thickness 450 - 700 mm |
60900 psi @Strain 0.200 %, Thickness 17.7 - 27.6 in |
long-transverse direction |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Tensile Strength, Yield | 420 MPa @Strain 0.200 %, Thickness 450 - 700 mm |
60900 psi @Strain 0.200 %, Thickness 17.7 - 27.6 in |
Typical Strength |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
Tensile Strength, Yield | >= 420 MPa @Strain 0.200 %, Thickness 50.0 - 100 mm |
>= 60900 psi @Strain 0.200 %, Thickness 1.97 - 3.94 in |
Temper T651 |
Constellium Certal® Thick Aluminum Plate Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and .. |
|||
Tensile Strength, Yield | >= 420 MPa @Strain 0.200 %, Thickness 60.0 - 80.0 mm |
>= 60900 psi @Strain 0.200 %, Thickness 2.36 - 3.15 in |
|
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |