Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Thickness 4.00 mm, Temperature -20.0 °C |
5.71 ft-lb/in² @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature 0.000 °C |
5.71 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 244R PC (Europe-Africa-Middle East) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also US FDA food contact compliant available in limited colorsThis dat.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE163R PC (Europe-Africa-Middle East) LEXAN FXE163R is a transparent/translucent UV stabilized, medium viscosity grade for special effects with fluorescent appearance. Color package may affect performance. LEXAN FXE163R contains a relea.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXM4701 PPC LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Americas .. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® VR2520 PC General purpose polycarbonate with melt flow rate of 8.5.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -18.0 °C |
5.71 ft-lb/in² @Temperature -0.400 °F |
10.0-mm x 4.0-mm, 0.25-mm notch; ISO 180 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC0703 PC PC0703 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC0800 PC PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC1000 PC PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC1000R PC PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC1800R PC PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC1800R PC (Asia Pacific) PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
5.71 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
5.71 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -20.0 °C |
5.71 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Dow INSPIRE™ 112 Performance Polymer INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -20.0 °C |
5.71 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG8 PA66, 40% Glass Fiber Reinforced, Injection Molding Staramide AG8 is a 40% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 NL IM PBT, unfilled, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR30 NL HW PA6, 30% glass fiber reinforced, hydrolysis stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -40.0 °C |
5.71 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 KK30 NL IL PA 6 30% glass fiber/mineral reinforced, impact modified, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |