Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 10.0 - 11.0 kJ/m²
4.76 - 5.23 ft-lb/in²
ASTM D256
Polikim EFALON® B-60 PTFE, 60% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
Izod Impact, Notched (ISO) 8.00 - 11.0 kJ/m²
3.81 - 5.23 ft-lb/in²
Average value: 9.20 kJ/m² Grade Count:5
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Izod Impact, Notched (ISO) 8.00 - 11.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 5.23 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.67 kJ/m² Grade Count:3
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Izod Impact, Notched (ISO) 4.90 - 11.0 kJ/m²
2.33 - 5.23 ft-lb/in²
Average value: 8.03 kJ/m² Grade Count:3
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Izod Impact, Notched (ISO) 3.00 - 11.0 kJ/m²

@Temperature -30.0 - 0.000 °C
1.43 - 5.23 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 5.71 kJ/m² Grade Count:13
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Izod Impact, Notched (ISO) 5.00 - 11.0 kJ/m²
2.38 - 5.23 ft-lb/in²
Average value: 7.67 kJ/m² Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Izod Impact, Notched (ISO) 2.00 - 11.0 kJ/m²

@Temperature -40.0 - -20.0 °C
0.952 - 5.23 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 6.00 kJ/m² Grade Count:17
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Izod Impact, Notched (ISO) 11.0 - 11.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.23 - 5.23 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 11.0 kJ/m² Grade Count:1
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched (ISO) 6.00 - 11.0 kJ/m²
2.86 - 5.23 ft-lb/in²
Average value: 8.13 kJ/m² Grade Count:3
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Izod Impact, Notched (ISO) 4.00 - 11.0 kJ/m²
1.90 - 5.23 ft-lb/in²
Average value: 8.26 kJ/m² Grade Count:31
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched (ISO) 6.00 - 11.0 kJ/m²
2.86 - 5.23 ft-lb/in²
Average value: 7.44 kJ/m² Grade Count:18
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..