Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON TE002 PU LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | ISO 180/1eA |
Lubrizol ESTALOC® T5160 Ether-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Starpylen HT 25 MC PP, Mineral Filled, Injection Molding Starpylen HT 25 MC is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | ISO 180/1A |
Total Lacqrene® 9218 Polystyrene
(discontinued **) LACQRENE® 9218 is a polystyrene modified with polyethylene. This combination gives a high level of stress crack resistance with excellent mechanical properties and good abrasion resistance. This .. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND PCA 839 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with very good impact behaviour even at low temperatures, good dimensional stability. Vicat/B50 = 130°C Main applications fields: a.. |
|||
Izod Impact, Notched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66 LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |