Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 10.0 - 11.0 kJ/m² | 4.76 - 5.23 ft-lb/in² | ASTM D256 |
Polikim EFALON® B-60 PTFE, 60% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Izod Impact, Notched (ISO) | 8.00 - 11.0 kJ/m² | 3.81 - 5.23 ft-lb/in² | Average value: 9.20 kJ/m² Grade Count:5 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched (ISO) | 8.00 - 11.0 kJ/m² @Temperature -30.0 - -30.0 °C |
3.81 - 5.23 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 9.67 kJ/m² Grade Count:3 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched (ISO) | 4.90 - 11.0 kJ/m² | 2.33 - 5.23 ft-lb/in² | Average value: 8.03 kJ/m² Grade Count:3 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 11.0 kJ/m² @Temperature -30.0 - 0.000 °C |
1.43 - 5.23 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 5.71 kJ/m² Grade Count:13 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 11.0 kJ/m² | 2.38 - 5.23 ft-lb/in² | Average value: 7.67 kJ/m² Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 11.0 kJ/m² @Temperature -40.0 - -20.0 °C |
0.952 - 5.23 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 6.00 kJ/m² Grade Count:17 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched (ISO) | 11.0 - 11.0 kJ/m² @Temperature -30.0 - -30.0 °C |
5.23 - 5.23 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 11.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 11.0 kJ/m² | 2.86 - 5.23 ft-lb/in² | Average value: 8.13 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Izod Impact, Notched (ISO) | 4.00 - 11.0 kJ/m² | 1.90 - 5.23 ft-lb/in² | Average value: 8.26 kJ/m² Grade Count:31 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched (ISO) | 6.00 - 11.0 kJ/m² | 2.86 - 5.23 ft-lb/in² | Average value: 7.44 kJ/m² Grade Count:18 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |