Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact, high heat and excellent extrusion and thermoforming characteristics. Halogen free.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS Reinforced PC/ABS with high stiffness and low CTE. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -40.0 - -40.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 20.0 kJ/m² Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, Conditioned Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 180/1A |
SYNTHOS Forsan® 573 L Acrylonitrile Butadiene Styrene (ABS) Increased heat resistant, glossy, UV stabilized.Applications: Electrotechnics, automotiveHousehold appliances, office equipment, car interior parts, profiles, ABS sheets, etc.Synthos was formerly kn.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Kalix® 2955 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2955 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is specifically formulated for high strength and stiffness applications where .. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Izod Impact, Notched (ISO) | >= 20.0 kJ/m² | >= 9.52 ft-lb/in² | |
Sibur ABS 2020-30M Molding Grade ABS Plastic With high thermal and light resistance for automobile building, stable to atmospheric conditions in thermal and electric ageing, contacting with food products, as well as with compounding with PC. |
|||
Izod Impact, Notched (ISO) | >= 20.0 kJ/m² | >= 9.52 ft-lb/in² | |
Styrolution Absolac® 300 ABS Standard impact gradeHigh flowInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermotuf PF007IX2 PA 6 (Europe-Africa-Middle East) LNP * THERMOTUF* PF007IX2 is a compound based on PA 6 resin containing Glass Fiber. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East) NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/A |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/A |
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 BK30564 is an impact-modified, pigmented black, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV006BS PP LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl.. |
|||
Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RVL36 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RVL36 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. |