Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East) LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific) LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXD PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXD is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Lubricomp ZFL36CCX PPE+PS LNP LUBRICOMP* ZFL36CCX is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF004ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific) LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008 |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific) LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP UF008AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF008AS is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Izod Impact, Notched (ISO) | >= 13.0 kJ/m² | >= 6.19 ft-lb/in² | |
Styrolution Absolac® 380 ABS High glossHigh flowInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | >= 13.0 kJ/m² | >= 6.19 ft-lb/in² | |
Styrolution Absolac® 700 ABS Very high glossInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp RF007S PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF007S is a compound based on PA 66 resin containing Glass Fiber . Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GFT33N051-NBK2 Nylon 66, 33% Glass Fiber Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GFX1743-BK1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6 Description: Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) 25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Star L POM D11 POM, Injection Molded Star L POM D11 is Silicone Oil Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Staramide R1000EI2 PA66, Impact Modified, Injection Molded Staramide R1000EI2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | ISO 180/A |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD4471 PC Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON LX04420C PEEK LNP* STAT-KON* LX04420C is a compound based on Polyetheretherketone resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding Syst.. |