Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180 |
PolyOne Nymax™ GBF 1010 35 BLACK 13 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | DIN 53453 |
Polikim ULPOLEN® 300 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature 0.000 °C |
5.71 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 101 PC (Europe-Africa-Middle East) LEXAN 101 is a high viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 101R PC (Europe-Africa-Middle East) LEXAN 101R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 101R is available in transparent, translucent and opaque colours. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 940A PC (Europe-Africa-Middle East) LEXAN 940A is a medium viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD103R PC FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP2R PC Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® IR1840 PC (Europe-Africa-Middle East) IR1840 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East) IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML3729 PC Excellent flow, UV stabilized, grade which contains a release agent to ensure easy processing. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC2203R PC (Europe-Africa-Middle East) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DX06094 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DX06094 is a compound based on Polycarbonate resin containing Glass Fiber . Added features include: High Impact, Non- Brominated & Non-Chlorinated Flame Retardant and Mold Release... |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® FX 4002 - UL94-V2 Flame Retardant Polypropylene Copolymer Compound with High Impact Strength V-2 Flame Retardant PP Copolymer with High Impact StrengthApplications: Battery LidsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF33A099-HRN Nylon 66, 33% Glass Reinforced, Hydrolysis Resistant All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Staramide AK8ST41 PA66, Mineral Reinforced, Impact Modified, Injection Molding Staramide AK8ST41 is an Impact Modified, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 12.0 - 12.0 kJ/m² @Temperature -40.0 - -40.0 °C |
5.71 - 5.71 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 12.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180 |
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD1647 PBT+PC (Europe-Africa-Middle East) XENOY XD1647 is a semi crystalline, impact modified PBT+PC blend, containing 15% mineral filler. It is especially developed to obtain a reduced coefficient of thermal expansion combined with good ch.. |