Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific) LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East) LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP JZL012 PES (Europe-Africa-Middle East) LNP* LUBRICOMP* JZL012 is a compound based on Polyethersulfone resin containing Proprietary Filler, PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP PDX-U-05314 PPA (Asia Pacific) LNP* Lubricomp* PDX-U-05314 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL34 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Asia Pacific) LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as Lub.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RN001XXC PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RN001XXC is a compound based on Nylon 66 resin containing MOS2. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON CX99000 PS (Europe-Africa-Middle East) LNP* STAT-KON* CX99000 is a compound based on Polystyrene containing Carbon Powder. Added features include : Electrically Conductive, Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East) VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON PX93058 PA 6 (Europe-Africa-Middle East) LNP*STATKON*PX93058 is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON SC004 PA 12 (Europe-Africa-Middle East) LNP* Stat-kon* SE004 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB55 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* WF006 is a compound based on Polybutylene Terephalate resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MV008 PP (Europe-Africa-Middle East) LNP* VERTON* MV008 is a compound based on Polypropylene resin containing Long Glass. Added features include Chemically Coupled. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MX05039 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MX05039 is a compound based on Polypropylene resin containing Mineral, colorant. Added features include : Heat- Stabilized, UV - Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA D51 PA6, Injection Molded Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF007ESS PA66/6, 35% Glass Filled, Injection Molded Staramide RF007ESS is a 35% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as RF1007EMHS)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 50.0 - 120 kJ/m² | 23.8 - 57.1 ft-lb/in² | Average value: 89.0 kJ/m² Grade Count:5 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |