Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 FRC 3 PA 66 basic type with flame retardant Features: Modified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. Used in automotive, electrical, engineering and .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Novodur® HH-106 ABS Novodur HH-106 is a high heat injection molding grade providing a balanced property profile.Information provided by Styrolution |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature 23.0 °C |
>= 47.6 ft-lb/in² @Temperature 73.4 °F |
NA; Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® M-1016 (Cond.) 33% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S223-HG6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Akulon® S223-PG8 PA66-GF40 40% Glass Reinforced, Impact Modified |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Starflam PX06004 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 GR30 NL IH PA 6.6 30% glass fiber reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV330 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 835T Acrylonitrile Butadiene Styrene Saxalac 835T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) Zytel® 70G35HSRX BK099 a 35% glass reinforced, heat stabilized, hydrolysis resistant PA66 for injection molding. Developed for applications designed for direct overmolding of gaskets onto thermopla.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Novamid® MC112LG55 C10 PA6-GF55 55% Glass Reinforced |