Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -20.0 °C |
23.8 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 26 B PA6 Basic type PA 6 for compounding, for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in the natural mode and in the full RAL color scale.Information Prov.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 GF 30 002 TS PA6 reinforced with glass fiber, heat stabilized PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used for holders of hand tools, hobby tools, gear wheel.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suita.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRB 4 Polyamide 6, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding with increased flammability resistance. Halogen-free flame retardant. Intended for electrical purposes. Manufacturing of simple large scale products. Good flo.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -20.0 °C |
23.8 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 30 006/1M PA6 reinforced with 30% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 30% of milled glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and cons.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -20.0 °C |
23.8 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnite® TV4 460 KL TV4 460 PBT/PET Blend-30% Glass Reinforced (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Arnite® AV2 370 /B AV2 370 PET-35% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® S223-PG6U (Cond.) 33% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued ** Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
LG Chemical LG-703A ABS, Low Gloss, General Purpose Information Provided by LG Chem |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 179-1eU |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow) |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 3225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Lanxess Durethan® BKY 115 H3.0 DUS008 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® BF 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® BF 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1fU |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Arnite® TV4 261 SF PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant, High Flow |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 GR30 NL CA 01 PBT/PET 30% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
LG Chemical HG-174 ABS, High Gloss, Super High Flow Information Provided by LG Chem |