Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | <= 40.0 MPa | <= 5800 psi | ISO/R527 |
Polykemi AB POLYabs V0X ABS, Flame Retardant Information provided by Polykemi AB |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY203 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY203 is a industrial quality PC+ABS flame retardant grade for injection moulding applications. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Europe-Africa-Middle East) PC+ABS, of non-chlorinated & non-brominated flame retardant with Sparkle effect.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | |
Radici Radilon® A CV300LK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Strength at Break | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Tensile Strength at Break | >= 40.0 MPa | >= 5800 psi | ISO.527 DN.53455 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Tensile Strength at Break | <= 40.0 MPa | <= 5800 psi | ISO/R527 |
Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | |
LATI Latilub 37 B01-02S Bio-Polymer Self-lubricating product based on Bio-Polymer (PLA, PHB, ...). Silicone.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | |
LATI Latistat 36/MR-04 ABS Dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | ISO 527 Type 1A |
Solvay TECHNYL® eXten D 458P PA6.10, DRY Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | ISO 527 |
Techmer ES Plaslube® NY-6/MS/M PA12 |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | ISO 527 Type 1A |
Solvay TECHNYL® A 208F PA66, Conditioned Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta.. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX1112 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1112 is an unfilled medium heat resistant material. This grade offers improved impact resistance to meet the ECE-dashboard standard. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Stat-loy W3000 PBT LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific) PPE+PS, HDT 125 |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | ISO 527 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Tensile Strength at Break | >= 40.0 MPa | >= 5800 psi | ASTM D638 |
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE. |
|||
Tensile Strength at Break | >= 40.0 MPa | >= 5800 psi | ASTM D638 |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 40 X PA12-I Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m.. |
|||
Tensile Strength at Break | 40.0 - 50.0 MPa | 5800 - 7250 psi | ASTM D638 |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 90 LXS PAMACM12 Product description: Grilamid TR 90 LXS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LXS natural contains a processing.. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | ISO R 527 |
Fainplast Compounds MRK 267 Medical Rigid PVC, Injection Molding Anti-impact connectors and components |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | ASTM D638 |
Bayshore Vinyl Compounds BRC R409002 Molding Compound BRC 409002 is a medium impact high flow injection molding compound designed for ease of process along with excellent weathering characteristics.Information Provided by Bayshore Vinyl Compounds Inc. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | 50mm/min; ASTM D638 |
3M Dyneon™ PVDF 6108/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | |
AorTech Biomaterials ECSil™ 70D Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | |
Radici Radilene® R 70 IF 0 4058 A High Density Polyethylene Shore hardness: 61 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a.. |
|||
Tensile Strength at Break | 40.0 MPa | 5800 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, Conditioned Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced .. |