Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polimersan Plastics
Trade Name POLIPOLEN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monomer, is polymerized by low pressure or high pressure method and then can be maintained as high density (PE-YY 0,941 and 0,965 g/cm³) or low (normal) density polyethylene(PE-NY 0,914 and 0,925 g/cm³). Other differences of various PE types are according to their melting degrees and opposite proportional connection occurs according to their relative molecular weights. In other words, when its melting degree is at the lowest level, its relative molecular weight is at the highest level and e.g. its mechanical specialties are the best.POLIPOLEN has quite a low density. Its flexibility rate is high and it is resistant to strokes even at low temperatures. It has a very high molecular weight(molecular chain length). It has a high corrosion resistance because of its high molecular chain. According to the results of the "sand slurry" corrosion test which is made as per "DIN" standards, POLIPOLEN 1000 , has shown the highest corrosion resistance among the solid materials( e.g. steels, tree, other engineering plastics.)PROPERTIES OF POLIPOLEN®:Very high stroke resistanceVery high corrosion resistanceVery high chemical resistanceGetting lubricated itself and slickExcellent electrical resistanceQuietness while processing and reducing vibrationsEasy processingLow friction rateVery low water absorptionGENERAL USAGE AREAS OF POLIPOLEN®:Coal warehouses and conveyor systemsGuttersChain conveyor guidesElevatorsElectric power stationsCement industryLime industryPalister industryFood industryCutting and chopping platesChopping blocksConveyor screwsSliding elementsFlat guidesProfilesBobbinsStar and screw conveyorsElevator systemsSliding bearingsGearsMotor landing platesStopper valvesClosing clapsAcid pumpsFilters Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.
Physical Properties Metric English Comments
Specific Gravity >= 0.950 g/cc
>= 0.950 g/cc
ISO.1183 DN.53479
Water Absorption <= 0.020 %
<= 0.020 %
ISO.62 DN.53495
Mechanical Properties Metric English Comments
Hardness, Shore D 60 - 70
60 - 70
DN.53505
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO.2039-2
Tensile Strength at Break >= 40.0 MPa
>= 5800 psi
ISO.527 DN.53455
Tensile Strength, Yield 20.0 - 25.0 MPa
2900 - 3630 psi
ISO.527 DN.53455
Elongation at Break >= 500 %
>= 500 %
ISO.527 DN.53455
Elongation at Yield 12 %
12 %
ISO.527 DN.53455
Modulus of Elasticity >= 0.800 GPa
>= 116 ksi
ISO.178 DN.53452
Charpy Impact, Notched 5.00 J/cm²
23.8 ft-lb/in²
ISO.179 DN.53453
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
DN.53752
Melting Point 130 - 133 °C
266 - 271 °F
Maximum Service Temperature, Air 70.0 °C
158 °F
ISO.75 DN.53461
Electrical Properties Metric English Comments
Volume Resistivity >= 5.00e+16 ohm-cm
>= 5.00e+16 ohm-cm
ISO.167 DN.53482
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO.167 DN.53482
Dielectric Strength >= 50.0 kV/mm
>= 1270 kV/in
ISO.243 DN.53481
Descriptive Properties Value Comments
Corrosion < 400 %
DN.58836 Sand Slurry Test