Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + Bright ESD Polyethylene, Conductive Material ”S”® plus+ Bright ESD is a light plastic with high conductivity and a voltage-dissipating effect on earthed components. This material is ideal for use in applications where a high value.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 82 N 003/1M Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | |
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 37 |
PolyOne OnFlex™ U 5370A-S0015 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of.. |
|||
Tensile Strength at Break | <= 25.0 MPa | <= 3630 psi | ISO/R527 |
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Tensile Strength at Break | >= 25.0 MPa | >= 3630 psi | DIN 53504 |
Huntsman AVALON® 75 ABX Thermoplastic Polyurethane Introduction: AVALON 70 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Tensile Strength at Break | 25.0 - 27.0 MPa | 3630 - 3920 psi | ASTM D683 |
Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | |
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |
|||
Tensile Strength at Break | >= 25.0 MPa | >= 3630 psi | |
Shandong Dongyue Shenzhou New Material Co DS601 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
SCG Chemicals EL-Proâ„¢ P401S Polypropylene Flat Yarn/Sheet Key Characteristics: Excellent mechanical propertiesRecommended Applications:Stretch tape for jumbo woven sheetMonofilament for rope and sheetInformation provided by SCG Chemicals |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
UBE V115 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
Total PS CPDS 818 Easy Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 818 is a high heat resistant, high impact Polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacturing of articles which r.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 527 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
Eastman Eastar MN021 Copolyester Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
Eastman Eastar MN200 Copolyester Eastar Copolyester MN200 is an amorphous copolyester with excellent flow characteristics as well as radiation resistance and chemical resistance.Applications/UsesMedical |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
Eastman TiGlaze SV Copolyester TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D 638 |
Cossa Polimeri ESTAPROP 1050 V0 HF H Flame Retardant Polypropylene PP homopolymerFlame retardant class V0, halogen free, excellent mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D 638 |
Cossa Polimeri ESTASTIR HI 0810 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, high impact resistance, good melt flow rate, good light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 527-1/-2 |
Covestro Desmopan® DP 9370AU Polyurethane Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission r.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 527-1/-2 |
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 527 |
Eurotec® Tecolen® CP20 BK EC PPCP, conductive, black Information provided by Eurotec® |
|||
Tensile Strength at Break | 25.0 MPa @Temperature 120 °C |
3630 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |
|||
Tensile Strength at Break | 25.0 MPa @Temperature 80.0 °C |
3630 psi @Temperature 176 °F |
ISO Data |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | |
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 527 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |