Material Notes:
Total Petrochemicals Polystyrene 818 is a high heat resistant, high impact Polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacturing of articles which require good dimensional stability at elevated temperatures.Suitable Applications for Total Petrochemicals Polystyrene 818 include TV covers, printers, scanners, electrical appliances.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Spiral Flow 57.0 cm

@Temperature 220 °C
22.4 in

@Temperature 428 °F
ASTM D3123
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D638
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 1.95 GPa
283 ksi
ASTM D638
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Vicat Softening Point 95.0 °C

@Load 1.02 kg
203 °F

@Load 2.25 lb
50°C per hour; ASTM D1525
Heat Distortion Temperature >= 78.9 °C
>= 174 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 2.10 mm
V-0

@Thickness 0.0827 in
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC 93
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149