Mechanical Properties Metric English Comments
Tensile Strength at Break 144 MPa
20900 psi
ISO 527
Nilit FRIANYL A63 W-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Strength at Break 144 MPa
20900 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK
LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength at Break 144 MPa
20900 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched
LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Tensile Strength at Break 144 MPa
20900 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS (Asia Pacific)
LNP* Lubricomp* OFL36A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength at Break 144 MPa
20900 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS
LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Tensile Strength at Break 144 MPa
20900 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics Ultem ATX153R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength at Break 144 MPa
20900 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Strength at Break 144 MPa
20900 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM CRS5211R PEI
20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming.
Tensile Strength at Break 144 MPa
20900 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM CRS5211R PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming.
Tensile Strength at Break 144 MPa
20900 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon EE002ER PEI (Europe-Africa-Middle East)
LNP* Lubricomp* EFP36G is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.This data wa..
Tensile Strength at Break 144 MPa
20900 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Tensile Strength at Break 144 MPa
20900 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Tensile Strength at Break 144 MPa
20900 psi
5 mm/min; ISO 527
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded
Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar.
Tensile Strength at Break 144 MPa
20900 psi
ISO 527
Azdel Plus C507-B01 50% Chopped Fiber Mat / PP Resin Matrix (Mineral filled)
AZDEL® C507-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu..
Tensile Strength at Break 144 MPa
20900 psi
ISO 527
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Conditioned)
Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio..
Tensile Strength at Break 144 MPa
20900 psi
ASTM D638
LNP Lubricomp® PDX-O-88533 BK8-229 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant  (disconti
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Copyright © lookpolymers.com All Rights Reserved