Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1100-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-10 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.99 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D4812 |
PolyOne Geon™ 81520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 3.20 J/cm - NB | 5.99 ft-lb/in - NB | Average value: 5.33 J/cm Grade Count:14 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON AE004 ABS LNP STAT-KON* AE004 is a compound based on ABS resin containing 20% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON AX06518 ABS (Asia Pacific) LNP* Stat-kon* AX06518 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, Fl.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 855 PBT 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific) 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Temperature 23.0 °C |
5.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp MF006ASJ PP LNP THERMOCOMP* MF006ASJ is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized, Healthcare.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Temperature -30.0 °C |
5.99 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East) 10% GF FR PBT/PC Blend |
|||
Izod Impact, Unnotched | 3.20 J/cm @Temperature -30.0 °C |
5.99 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Temperature -30.0 °C |
5.99 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66 (Asia Pacific) LNP* Thermocomp* RB006 is a compound based on Nylon 66 resin containing Glass Bead. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Adell EL-16 Homopolymer Polypropylene, 30% Mineral Filled; Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 102 Polypropylene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | Method A; ASTM D256 |
Proto3000 PC Fused Deposition Modeling Polymer Description: A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating .. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis.. |
|||
Izod Impact, Unnotched | 3.20 - 8.54 J/cm @Temperature -40.0 - -40.0 °C |
5.99 - 16.0 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 5.00 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Temperature 23.0 °C |
5.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp UC008S PPA LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |