Material Notes:
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Water Absorption 0.060 %
<br>@Time 86400 sec
0.060 %
<br>@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
<br>@Thickness 1.50 - 3.20 mm
0.0040 - 0.0060 in/in
<br>@Thickness 0.0591 - 0.126 in
SABIC Method
0.0060 - 0.0090 cm/cm
<br>@Thickness 3.20 - 4.60 mm
0.0060 - 0.0090 in/in
<br>@Thickness 0.126 - 0.181 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm
<br>@Thickness 1.50 - 3.20 mm
0.0050 - 0.0080 in/in
<br>@Thickness 0.0591 - 0.126 in
SABIC Method
0.0080 - 0.011 cm/cm
<br>@Thickness 3.20 - 4.60 mm
0.0080 - 0.011 in/in
<br>@Thickness 0.126 - 0.181 in
SABIC Method
Melt Flow 81 g/10 min
<br>@Load 5.00 kg,<br> Temperature 266 °C
81 g/10 min
<br>@Load 11.0 lb,<br> Temperature 511 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength at Break 89.0 MPa
12900 psi
Type I, 5 mm/min; ASTM D638
Flexural Strength 137 MPa
19900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 45.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
61.2 µm/m-°C
<br>@Temperature 60.0 - 138 °C
34.0 µin/in-°F
<br>@Temperature 140 - 280 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 204 °C
<br>@Thickness 6.40 mm
399 °F
<br>@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 187 °C
<br>@Thickness 6.40 mm
369 °F
<br>@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 125 °C
257 °F
UL 746B
UL RTI, Mechanical with Impact 110 °C
230 °F
UL 746B
UL RTI, Mechanical without Impact 125 °C
257 °F
UL 746B
Flammability, UL94 V-0
<br>@Thickness 1.47 mm
V-0
<br>@Thickness 0.0579 in
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 4.50e+16 ohm-cm
4.50e+16 ohm-cm
ASTM D257
Dielectric Constant 3.4
<br>@Frequency 1.00e+6 Hz
3.4
<br>@Frequency 1.00e+6 Hz
ASTM D150
3.5
<br>@Frequency 100 Hz
3.5
<br>@Frequency 100 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
<br>@Thickness 3.20 mm
508 kV/in
<br>@Thickness 0.126 in
in air; ASTM D149
22.4 kV/mm
<br>@Thickness 1.60 mm
569 kV/in
<br>@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor 0.0010
<br>@Frequency 100 Hz
0.0010
<br>@Frequency 100 Hz
ASTM D150
0.010
<br>@Frequency 1.00e+6 Hz
0.010
<br>@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
0.00 - 15 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
UL 746A
Descriptive Properties Value Comments
Specific Volume 0.65cm^3/g
ASTM D792