Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded
&nbs AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance mol.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and .. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Izod Impact, Unnotched | 5.30 J/cm @Thickness 3.18 mm |
9.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP PF003 PA 6 LNP THERMOCOMP* PF003 is a compound based on Nylon 6 resin containing 15% Glass Fiber. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Unnotched | 5.30 J/cm @Temperature -30.0 °C |
9.93 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Unnotched | 5.30 J/cm @Temperature -30.0 °C |
9.93 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Unnotched | 5.30 J/cm @Temperature -30.0 °C |
9.93 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |