| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
| Water Absorption | 0.030 % | 0.030 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 57 | 57 | ASTM D785 |
| Hardness, Rockwell R | 105 | 105 | ASTM D785 |
| Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | ASTM D638 |
| Elongation at Break | 7.0 % | 7.0 % | ASTM D638 |
| Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
| Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
| Izod Impact, Notched | 1.20 J/cm | 2.25 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
| Gardner Impact | 0.800 J | 0.590 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 160 °C | 320 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 309 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 146 °C | 295 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |