Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
7.49 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Maxxam™ PPH-40C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm |
7.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Izod Impact, Unnotched | 4.00 - 5.07 J/cm | 7.50 - 9.50 ft-lb/in | Average value: 4.36 J/cm Grade Count:3 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® ABS GF30 FR 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 1018121Information provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GM30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Temperature -30.0 °C |
7.49 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Spartech SP-9010 General Purpose ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF30 HT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC LNP* THERMOCOMP* DB008ERP is a compound based on Polycarbonate resin containing 40% Glass Bead. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC (Asia Pacific) LNP* Thermocomp* DB008ERP is a compound based on Polycarbonate resin containing Glass Bead. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 413 Polyester - PBT, Glass Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® ABS/PBT GF15 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications. |