Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
ISO 179
PolyOne LubriOne™ NN-30CF/15T-02S black Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
ISO 11542-2
Okulen® 1000 PE-UHMW, Natural
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Charpy Impact Unnotched 2.10 J/cm²

@Temperature -40.0 °C
9.99 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.10 - 8.50 J/cm²

@Temperature -40.0 - -20.0 °C
9.99 - 40.5 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.82 J/cm² Grade Count:4
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing
Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG
Charpy Impact Unnotched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 20-8254 Polyphthalamide, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Charpy Impact Unnotched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK Polycarbonate, with carbon fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Charpy Impact Unnotched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 50-7078/GY Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® ST15G6 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
Complete Break; ISO 179
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral
Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater..
Charpy Impact Unnotched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® 388 S SAN
Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
ISO 179
Vyncolit X6952 Novolac Phenolic
Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn..
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
ISO 179
Chi Mei Kibisan® PN-127 SAN
Heat Resistant
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers
Charpy Impact Unnotched 2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 3520 L Polypropylene
Grade containing antiblocking agent; sealing layer for OPP film.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
Biomer P209 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Charpy Impact Unnotched 2.10 - 8.00 J/cm²
9.99 - 38.1 ft-lb/in²
Average value: 5.82 J/cm² Grade Count:18
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Charpy Impact Unnotched 2.10 - 4.00 J/cm²

@Temperature -30.0 - 30.0 °C
9.99 - 19.0 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 2.90 J/cm² Grade Count:10
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
Charpy Impact Unnotched 2.10 - 6.50 J/cm²
9.99 - 30.9 ft-lb/in²
Average value: 4.59 J/cm² Grade Count:15
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Charpy Impact Unnotched 2.10 - 6.50 J/cm²

@Temperature -30.0 - -30.0 °C
9.99 - 30.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.62 J/cm² Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Copyright © lookpolymers.com All Rights Reserved