Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | ISO 179 |
PolyOne OnForce™ LFT NY-50LGF/001 HS Natural Polyamide 6 (Nylon 6) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 50/TF/15/BK7284 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Europe-Africa-Middle East) UV stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | ISO 179 |
Polyram Polytron P50N07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced natural polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® AG-35 PA66-GF35 Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 CF 18 HWCP 18% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW200F8 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW200F8 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65 Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65 Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-35/4 PA666-GF35 Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4108 black 9992 PA612-GF50 Product description: Grilamid XE 4108 black 9992 is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorpti.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® FG70G30HSR3 BK309 Nylon 66
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 PA6-GF50 Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60 Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl A2 V40 Nylon 66, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | |
BASF Procom® D 1188 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |