Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179-1 |
Polycasa PS QUINN PS sheets have good optical properties and a brilliant surface. The QUINN PS range contains sheets that are easy to fabricate, to vacuum form, and show a high light transmission (min 88% wavel.. |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² @Temperature 23.0 °C |
2.86 - 3.81 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 572R Phenolic Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, As Conditioned
(discontinued **) Standard injection molding grade, easy flow, easy mold release, fast setting.Applications: Thin walled engineering parts. Automotive sector: air filters, switch and connector parts for car electric... |
|||
Charpy Impact Unnotched | 0.600 - 1.70 J/cm² | 2.86 - 8.09 ft-lb/in² | Average value: 1.12 J/cm² Grade Count:5 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® 1465, Injection Grade
(discontinued **) Injection molding grade, increased heat resistance and flow, high gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires .. |
|||
Charpy Impact Unnotched | 0.600 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
2.86 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.813 J/cm² Grade Count:19 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact Unnotched | 0.600 - 8.60 J/cm² | 2.86 - 40.9 ft-lb/in² | Average value: 3.69 J/cm² Grade Count:28 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Charpy Impact Unnotched | 0.600 - 1.36 J/cm² | 2.86 - 6.47 ft-lb/in² | Average value: 0.889 J/cm² Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application .. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² | 2.86 ft-lb/in² | |
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² | 2.86 - 3.81 ft-lb/in² | ISO 179 |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9371 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated .. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnitel® UM552 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, Dry as Molded
(discontinued **) Injection molding grade, higher stiffness, good stress corrosion cracking resistance and chemical resistance (fuel, cleaning agents).Information provided by Bayer.LANXESS was spun-off from Bayer in .. |
|||
Charpy Impact Unnotched | 0.600 J/cm² - NB | 2.86 ft-lb/in² - NB | Average value: 1.30 J/cm² Grade Count:4 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact Unnotched | >= 0.600 J/cm² @Temperature 23.0 °C |
>= 2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne Gravi-Tech™ GRV-NY-060-CU Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² | 2.86 - 3.81 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |