Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.80 J/cm² @Temperature -30.0 °C |
18.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL A63 GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HS-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² @Temperature -40.0 °C |
18.1 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 H-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² - NB | 18.1 ft-lb/in² - NB | Average value: 8.46 J/cm² Grade Count:171 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Charpy Impact Unnotched | 3.80 - 17.0 J/cm² | 18.1 - 80.9 ft-lb/in² | Average value: 10.1 J/cm² Grade Count:6 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7969 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² @Temperature -30.0 °C |
18.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 20-0665 Polyphthalamide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² @Temperature -30.0 °C |
18.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Europe-Africa-Middle East) PPX7110 is an alloy of PP and PPO, providing high impact and good heat resistance. Generic identification acc. ISO11469: >PP+PPE+PS-I |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | IS0179 |
Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | dry; ISO 179 |
Ter Hell Plastic Terez® PBT 7100 GF 30 Polybutylene Terephthalate, 30% Glass Fiber Description: PBT, 30% glass fiber reinforced.Application: Suitable for injection molding applications.Information provided by Ter Hell Plastic GMBH. |
|||
Charpy Impact Unnotched | 3.80 J/cm² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Crastin® SK692FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTNFG52G35HSL BK011 is a 35% glass reinforced lubricated heat stabilized high performance polyamide resin developed for consideration into a.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addilene H 590 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 302-G30 PBT Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 3.80 - 3.80 J/cm² @Temperature -20.0 - -20.0 °C |
18.1 - 18.1 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 3.80 J/cm² Grade Count:1 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Charpy Impact Unnotched | 3.80 - 9.00 J/cm² | 18.1 - 42.8 ft-lb/in² | Average value: 6.26 J/cm² Grade Count:30 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Charpy Impact Unnotched | 3.80 - 3.80 J/cm² @Temperature -30.0 - -30.0 °C |
18.1 - 18.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.80 J/cm² Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 3.80 - 8.20 J/cm² @Temperature -30.0 - -20.0 °C |
18.1 - 39.0 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 5.43 J/cm² Grade Count:27 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |