Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne LubriOne™ NN-25GB/15T Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 - 2.80 J/cm² @Temperature -30.0 - -30.0 °C |
13.3 - 13.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 2.80 J/cm² Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1850-7784 PBT, with glass fiber, glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BFG10-BN00N1 Nylon 6 10% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | EN ISO 179/1eU |
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | |
Covestro Baydur® GS PIR B Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GS 25 HWCP 25% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Charpy Impact Unnotched | 2.80 - 5.00 J/cm² | 13.3 - 23.8 ft-lb/in² | Average value: 4.14 J/cm² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Charpy Impact Unnotched | 2.80 - 8.60 J/cm² @Temperature -40.0 - -30.0 °C |
13.3 - 40.9 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.50 J/cm² Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Charpy Impact Unnotched | 2.80 - 5.30 J/cm² | 13.3 - 25.2 ft-lb/in² | Average value: 4.40 J/cm² Grade Count:24 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Charpy Impact Unnotched | 2.80 - 5.30 J/cm² @Temperature -30.0 - -20.0 °C |
13.3 - 25.2 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.68 J/cm² Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |