Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | ISO 179 |
PolyOne LubriOne™ NN-30CF/15T-02S black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | ISO 11542-2 |
Okulen® 1000 PE-UHMW, Natural OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -40.0 °C |
9.99 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.10 - 8.50 J/cm² @Temperature -40.0 - -20.0 °C |
9.99 - 40.5 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.82 J/cm² Grade Count:4 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 20-8254 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50-7078/GY Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® ST15G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | Complete Break; ISO 179 |
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® 388 S SAN Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | ISO 179 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | ISO 179 |
Chi Mei Kibisan® PN-127 SAN Heat Resistant |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3520 L Polypropylene Grade containing antiblocking agent; sealing layer for OPP film.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | |
Biomer P209 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Charpy Impact Unnotched | 2.10 - 8.00 J/cm² | 9.99 - 38.1 ft-lb/in² | Average value: 5.82 J/cm² Grade Count:18 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact Unnotched | 2.10 - 4.00 J/cm² @Temperature -30.0 - 30.0 °C |
9.99 - 19.0 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 2.90 J/cm² Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² | 9.99 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Charpy Impact Unnotched | 2.10 - 6.50 J/cm² | 9.99 - 30.9 ft-lb/in² | Average value: 4.59 J/cm² Grade Count:15 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Charpy Impact Unnotched | 2.10 - 6.50 J/cm² @Temperature -30.0 - -30.0 °C |
9.99 - 30.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.62 J/cm² Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |