Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Glass-reinforced Vydyne resins provide higher heat distortion temperature, resistance to creep and better dimensional stability when compared with unreinforced PA66. These products have good chemical resistance to a broad range of chemicals including gasoline, hydraulic fluids and most solvents. Vydyne R533 NT resin has tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy consumption and part weight are key advantages to Vydyne glass-fiber reinforced PA66 resins over aluminum and/or zinc die-cast parts. Typical Applications/End Uses: Vydyne R533 NT resin has been used for many under-the-hood automotive applications, motor housings for power tools and garden appliances. These resins have also been used in miscellaneous brackets, gears and clips that require high rigidity and strength.Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 33% Filler by WeightAdditive:Lubricant Features: Good Mold ReleaseHigh FlowHigh RigidityHigh StrengthLubricatedUses:Automotive Under the HoodGearsHousingsPower/Other Tools Appearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Diameter 2.00 mm
0.0040 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Diameter 2.00 mm
0.0090 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 145 MPa
21000 psi
ISO 527-2
Elongation at Break 5.0 %
5.0 %
ISO 527-2
Tensile Modulus 7.90 GPa
1150 ksi
ISO 527-2
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 6.50 GPa
943 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 180
14.0 kJ/m²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 8.50 J/cm²

@Temperature -30.0 °C
40.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179
1.40 J/cm²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 179