Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.40 J/cm² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6 GF 40 HI PA6 reinforced with glass fiber, improved impact strength PA 6 for injection molding, reinforced with 40% glass fiber, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East) CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A12^ F50 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANMID 6 B12^ F30 AS Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANMID 6 B43^ D F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific) Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® IFX6420Z PC (Asia Pacific) Lexan* IFX6420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ2220 PC Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ4320 PC (Europe-Africa-Middle East) LEXAN OQ4320 is a medium viscosity grade with a UV cut-off up to 400 nm and a greater optical purity than standard grades. Fields of application for this material are optical lenses, f.i. in sunglas.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -40.0 °C |
6.66 ft-lb/in² @Temperature -40.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 136F4Q32 Nylon 6, 20% Glass Fiber SAXAMID 136F4Q32 is a high impact-modified polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-HG7 (Dry) 35% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Novamid® 1015GH35 BK37 PA6-GF35 35% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPHC EP1001F Polypropylene Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |