Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PQ 81 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYshine PBT D241 PBT, Impact Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® 244R PC (Europe-Africa-Middle East) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also US FDA food contact compliant available in limited colorsThis dat.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® EX1036T PC (Europe-Africa-Middle East) LEXAN EX1036T is a transparent, high viscosity, UV stabilized polycarbonate grade and contains a release agent to ensure easy processing. LEXAN EX1036T is produced under tight color specifications.T.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® FXE101 PC (Europe-Africa-Middle East) Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-PG6U (Dry) 33% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **)&l Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3110 TO BU 10% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-3110 TO BU is a 10% talc-filled, black colored and UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3110 TO BU is developed for producing injection mol.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical SH-610 ABS, Extrusion, High Impact Information Provided by LG Chem |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179-1eA |
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers PA 6-Copolymer, 15% glass fibers, injection molding, impact modified |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 206 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Terluran® SP-6 ABS Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO R179 |
Styron Pulse® A35-110 PC/ABS PULSE™ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 12.0 °C |
16.7 ft-lb/in² @Temperature 53.6 °F |
ISO 179/1eA |
Styron CALIBREâ„¢ 303-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis BA204E Polypropylene Block Copolymer for Non-Pressure Pipes BA204E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA204E is recommended for non-pressure pipes & fittings, thin-walle.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® F223-D (Cond.) Low/Medium Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Akulon® K125/A PA6 Low Viscosity |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 NL IL PA 6.6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, Conditioned Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |