Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 27 B PA66 PA66 for compounding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, h.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 32 A PA66 PA66 basic type for injection molding, compounding, extrusion. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivere.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT SD PA66 Basic type PA66 for injection molding, modified for general use. PA66 contains TiO2 up to 0.5% wt. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners,.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT SD PA66 Basic type PA66 for injection molding, modified for general use. PA66 contains TiO2 up to 0.5% wt. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners,.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRB 4 Polyamide 6, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding with increased flammability resistance. Halogen-free flame retardant. Intended for electrical purposes. Manufacturing of simple large scale products. Good flo.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRM1X3 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 10 TS PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 178 |
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GB 20 LS PA66, 20% glass beads, light stability FeaturesPA 66 for injection moulding, chemically reinforced with 20 % glass beads, light stabilized, suitable for high strength and high impacted mouldings. Used in automotive, engineering and elect.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 T 40 FRO 3 PA66, 40% mineral filling, flame retardant FeaturesPA 66 with the content of 40% chemically modified mineral filling a with fire retardant. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produ.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTYR® B BT N PBT Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T15040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Qualchem Danamid FE Polyamide 6 Standard type polyamide with good flowing propertiesInformation provided by Qualchem Zrt. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Qualchem Danamid FEHUV Polyamide 6 Heat and UV stabilized, for long-lasting use at 120-130°C, protected against artificial lightInformation provided by Qualchem Zrt. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 4-8000 Polypropylene Random Copolymer INNOPOL® CS 4-8000 is a polypropylene random copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 4-8000 is highly suitable for pressure pipe manufacturing, includi.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
|
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis RA130E-6015 Polypropylene Random Copolymer RA130E-6015 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 81 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS15030 D Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 91 C 20 PP, 20% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |