Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GF 30 FRG 5 PA66, 30% glass fibre, flame retarder FeaturesPA 66 for injection moulding, chemically reinforced with 30 % glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /0,8 mm/ in accordance with .. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® GPM5500S ABS (Europe-Africa-Middle East) CYCOLAC GPM5500S is a multi purpose injection moulding grade, equal to GPM5500 but equiped with anti static agents, providing a favourable balance of engineering properties. CYCOLAC GPM5500S has a w.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYabs N20 ABS Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A43^E F14 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANMID 6 B32^ E F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANMID 6 B32^ EF F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 93 T 15 1/M PP, 15% mineral filling, UV stability FeaturesModified PP for injection moulding with the content of 15 % mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYabs F20 UV4 ABS, UV-stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RV300R (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical HT-700 ABS, High Strength, High Scratch Resistance Information Provided by LG Chem |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1e |
Aardvark Polymers AARTEL® 1000 Rotational Molding Resin Aartel 1000 is our premium grade of toughened impact modified acetal copolymer. Aartel 1000 is formulated with high impact properties combined with extended mechanical properties and elevated resist.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax BTG25-FN09N1 Nylon 6 25% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Novodur® E401 ABS Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® H702 ABS Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers |
|||
Charpy Impact, Notched | 1.60 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 GR40 NL PA 6.6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® A3K Q603 PA66 (Conditioned) Description: Ultramid A3K Q603 is a general purpose PA6/6.Information provided by BASF |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K223-P2 Impact Modified Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A RV500 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |