Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 69 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC T4030 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -20.0 °C |
<= 4.76 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Qualchem Danamid AFGF-20 Polyamide 66, 20% Glass Fiber Reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® ST820 BK503 PBT
(Unverified Data**) Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 179-1eA |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 179-1eA |
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced PA 6-Copolymer, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 179-1eA |
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Lanxess Pocan® B 1100 000000 PBT PBT, non-reinforced, extrusion, injection molding, improved flowability |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
Lanxess Pocan® ECO T 3220 000000 PBT + PET, 20% Glass Fiber PBT + PET, 20% glass fibers, injection molding, improved surface finish, contains 28% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66 PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Lanxess Durethan® AKV 15 000000 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K225-KWS Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-G4U (Cond.) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-G6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnite® AV2 365 SN PET-30% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
DIN ISO 179 |
BASF Elastollan R 2006 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® F223-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A RV400 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Stanyl® TE300 PA46 Heat Stabilized |